trained and understand gun-to-target distance. A manual gun
can be moved in to reach inside corners but not too close and
keep micro-amps lower when tight to the part surface.
Orange peel can be caused by excessive film thickness.
While this is true to a certain extent, a contributing factor is
electrostatic behavior. The film starts to increase resistance
by "insulating" the part surface. This causes a drop off in
film development with an increase in larger particle deposi-
tion and a reduction in smaller particle size deposition. The
increase in resistance can generate more rapid back-ioniza-
tion. So be aware of the role that film thickness has on the
back-ionization issue and avoid too much thickness.
POWDER BOOTHS
P R OV I D E D BY R O H N E R
Please call 888.885.7641 or visit rohnerpowderbooths.com
Spray to Waste Batch Recovery / Reclaim Process
Spray Booths Powder Booths Large Equipment Systems Ovens & Controls Custom Finishing Solutions
PRODUCTS FINISHING — PFonline.com
45
POWDER COATING
C L I N I C